Reinforced Electrode Architecture for a Flexible Battery with Paperlike Characteristics

Author(s): Gaikwad, Abhinav M; Chu, Howie N; Qeraj, Rigers; Zamarayeva, Alla M; Steingart, Daniel A

Download
To refer to this page use: http://arks.princeton.edu/ark:/88435/pr1pg50
Full metadata record
DC FieldValueLanguage
dc.contributor.authorGaikwad, Abhinav M-
dc.contributor.authorChu, Howie N-
dc.contributor.authorQeraj, Rigers-
dc.contributor.authorZamarayeva, Alla M-
dc.contributor.authorSteingart, Daniel A-
dc.date.accessioned2021-10-08T20:18:38Z-
dc.date.available2021-10-08T20:18:38Z-
dc.date.issued2013-02-10en_US
dc.identifier.citationGaikwad, Abhinav M., Howie N. Chu, Rigers Qeraj, Alla M. Zamarayeva, and Daniel A. Steingart. "Reinforced electrode architecture for a flexible battery with paperlike characteristics." Energy Technology 1, no. 2‐3 (2013): 177-185. doi: 10.1002/ente.201200027en_US
dc.identifier.urihttps://www.academia.edu/2188829/Reinforced_Electrode_Architecture_for_Flexible_Batteries_with_Paper-Like_Characteristics-
dc.identifier.urihttp://arks.princeton.edu/ark:/88435/pr1pg50-
dc.description.abstractCompliant energy storage has not kept pace with flexible electronics. Herein we demonstrate a technique to reinforce arbitrary battery electrodes by supporting them with mechanically tough, low‐cost fibrous membranes, which also serve as the separator. The membranes were laminated to form a full cell, and this stacked membrane reinforcement bears the loads during flexing. This technique was used to make a high energy density, nontoxic Zn–MnO2 battery with printed current collectors. The Zn and MnO2 electrodes were prepared by using a solution‐based embedding process. The cell had a nominal potential of 1.5 V and an effective capacity of approximately 3 mA h cm−2. We investigated the effect of bending and fatigue on the electrochemical performance and mechanical integrity of the battery. The battery was able to maintain its capacity even after 1000 flex cycles to a bend radius of 2.54 cm. The battery showed an improvement in discharge capacity (ca. 10 %) if the MnO2 electrode was flexed to tension as a result of the improvement of particle‐to‐particle contact. In a demonstration, the flexible battery was used to power a light‐emitting diode display integrated with a strain sensor and microcontroller.en_US
dc.format.extent177 - 185en_US
dc.language.isoen_USen_US
dc.relation.ispartofEnergy Technologyen_US
dc.rightsAuthor's manuscripten_US
dc.titleReinforced Electrode Architecture for a Flexible Battery with Paperlike Characteristicsen_US
dc.typeJournal Articleen_US
dc.identifier.doidoi:10.1002/ente.201200027-
dc.identifier.eissn2194-4296-
pu.type.symplectichttp://www.symplectic.co.uk/publications/atom-terms/1.0/journal-articleen_US

Files in This Item:
File Description SizeFormat 
ReinforceElectrodeFlexibleBattery.pdf2.89 MBAdobe PDFView/Download


Items in OAR@Princeton are protected by copyright, with all rights reserved, unless otherwise indicated.